Effect of Pre-Added HfO2 Inclusions on Carbide Morphology and Deformation Behavior in DZ125 Nickel-Based Superalloy

okfbejghlqji
Inclusions are important phases affecting material properties in complicated ways. In this paper. a quantitative study of the addition of HfO2 inclusions to DZ125 nickel-based superalloys was performed. Experimental results showed that the introduction of HfO2 inclusions caused a loss of strength and ductility. https://poolsproductscanadas.shop/product-category/aqua-genie-skimmer-parts/